Technical data for Wire and rods for oil and gas fasteners (ASTM A193, 194, A320)

Images: LOG IN | ACTIVATE NOW YOUR FREE ACCOUNT, COSTLESS
INFORMATION RESTRICTED TO THE REGISTERED USERS: LOG IN | ACTIVATE NOW YOUR FREE ACCOUNT, COSTLESS
INFORMATION RESTRICTED TO THE REGISTERED USERS: LOG IN | ACTIVATE NOW YOUR FREE ACCOUNT, COSTLESS
CLOSE

Wire and rods for oil and gas fasteners (ASTM A193, 194, A320)

Images: LOG IN | ACTIVATE NOW YOUR FREE ACCOUNT, COSTLESS
INFORMATION RESTRICTED TO THE REGISTERED USERS: LOG IN | ACTIVATE NOW YOUR FREE ACCOUNT, COSTLESS

Dati Tecnici/Technical Data/Technische Daten/Donné/Datos:
ASTM A193 - A320 Chemical requirements (Composition. percent)
ALLOY ASTM AISI UNS W.-Nr. Dia. Tensile strength min. MPa Yeld Strength min.0.2% MPa Elongation in 4 D. min.% Reduction of area min.% HB C Mn max P max S max Si max Cr Ni Mo V Ti Al max Cb+Ta
B5 A193 501 S50100 1.7362 up to 4.incl 690 550 16 50 - 0.10 min 1.00 0.04 0.03 1.00 4.00-6.00 - 0.40-0.65 - - - -
B6 A193 410 S41000 1.4006 up to 4.incl 760 585 15 50 - 0.15 min 1.00 0.04 0.03 1.00 11.5-13.5 - - - - - -
B7 A193 4140 G41400 1.7225 21/2 and under 860 720 16 50 <321 0.37-0.49 0.65-1.10 0.04 0.04 0.15-0.35 0.80-1.15 - 0.50-0.65 0.25-0.35 - 0.015 -
over 21/2 to 4 795 655 16 <302
over 4 to 7 690 515 18 <277
B7 M A193 4140 G41400 1.7225 21/2 and under 690   18 50 <235 0.37-0.49 0.65-1.10 0.04 0.04 0.15-0.35 0.80-1.15 - 0.50-0.65 0.25-0.35 - 0.015 -
over 21/2 to 4
over 4 to 7
L7 A320 4140 G41400 1.7225 21/2 and under 860 725 16 50 <235 0.38-0.48 0.75-1.00 0.04 0.04 0.15-0.35 0.80-1.10 - 0.15-0.25 - - - -
L7M A320 4140 G41400 1.7225 all size 690 550 18 50 0.38-0.48 0.75-1.00 0.04 0.04 0.15-0.35 0.80-1.10 - 0.15-0.25 - - - -
L43 A320 4340 G43400 1.6565 4 and under 860 725 16 50 0.38-0.43 0.60-0.85 0.04 0.04 0.15-0.35 0.70-0.90 1.65-2.00 2.0-3.0 - - - -
B8 A193 304 S30400 1.4301 all size 515 205 30 50 <223 0.08 max 2.00 0.05 0.03 1.00 18.0-20.0 8.0-11.0 - - - - -
A320 35
B8A A193 304 S30400 1.4301 all size 515 205 30 50 <192 0.08 max 2.00 0.05 0.03 1.00 18.0-20.0 8.0-11.0 - - - - -
A320 35
B8T A193 321 S32100 1.4541 all size 515 205 30 50 <223 0.08 max 2.00 0.05 0.03 1.00 17.0-19.0 9.0-12.0 - - 5xC min - -
A320 35
B8TA A193 321 S32100 1.4541 all size 515 205 30 50 <192 0.08 max 2.00 0.05 0.03 1.00 17.0-19.0 9.0-12.0 - - 5xC min - -
A320 35
B8C A193 347 S34700 1.4550 all size 515 205 30 50 <223 0.08 max 2.00 0.05 0.03 1.00 17.0-19.0 9.0-12.0 - - - - 10xC min
A320 35
B8CA A193 347 S34700 1.4550 all size 515 205 30 50 <192 0.08 max 2.00 0.05 0.03 1.00 17.0-19.0 9.0-12.0 - - - - 10xC min
A320 35
B8M A193 316 S31600 1.4401 all size 515 205 30 50 <223 0.08 max 2.00 0.05 0.03 1.00 16.0-18.0 10.0-14.0 2.0-3.0 - - - -
A320 35
B8MA A193 316 S31600 1.4401 all size 515 205 30 50 <192 0.08 max 2.00 0.05 0.03 1.00 16.0-18.0 10.0-14.0 2.0-3.0 - - - -
A320 35
B8cl2 A193 304 S30400 1.4301 3/4 and under 860 690 12 35 <321 0.08 max 2.00 0.05 0.03 1.00 18.0-20.0 8.0-11.0 - - - - -
A320
B8Tcl2 A193 321 S32100 1.4541 over 3/4 to 1 795 550 15 35 <321 0.08 max 2.00 0.05 0.03 1.00 17.0-19.0 9.0-12.0 - - 5xC min - -
A320 725 450 20
B8Ccl2 A193 347 S34700 1.4550 over 1 to 11/4 725 450 20 35 <321 0.08 max 2.00 0.05 0.03 1.00 17.0-19.0 9.0-12.0 - - - - 10xC min
A320 795 550 15
A193 347 S34700 1.4550 over 11/4 to 11/2 690 345 28 45
A320
B8Mcl2 A193 316 S31600 1.4401 3/4 and under 760 665 15 45 <321 0.08 max 2.00 0.05 0.03

1.00

16.0-18.0 10.0-14.0 2.0-3.0 - - - -
A320
A193 316 S31600 1.4401 over 3/4 to 1 690 550 20
A320
A193 316 S31600 1.4401 over 1 to 11/4 655 450 25
A320
A193 316 S31600 1.4401 over 11/4 to 11/2 620 345 30
A320
B8Mcl2B A193 316 S31600 1.4401 2 and under 655 515 25 40 <321                        
over 2 to 21/2 620 450 30
over 21/2 to 3 550 380 30
B8Mcl2C A193 316 S31600 1.4401 2 and under 585 450 30 60 <321                        
over 2 585 415 30                        
ASTM A 194 Chemical requirements (Composition. percent)
ALLOY ASTM AISI UNS W.-Nr. Dia. HB HRC HRB C Mn max P max S max Si max Cr Ni Mo V Ti Al max Cb+Ta
2 A194 1040 K04002 1.1191 all size 159 to 327 - - 0.40 min 1.00 0.04 0.05 0.40 - - - - - - -
2H A194 1040 K04002 1.1191 11/2 and under 248 to 327 24 to 28 -
over 11/2 212 to 327 38 max 95 min
2HM A194 1040 K04002 1.1191 all size 159 to 327 22 max -
4L A194 - K14510 - all size 248 to 327 24 to 38 - 0.40 - 0.50 0.70 - 0.90 0.035 0.04 0.15 - 0.35 - - 0.20 - 0.30 - - - -
3 A194 501 S50100 1.7362 all size 248 to 327 24 to 38 - 0.10 min 1.00 0.04 0.03 1.00 4.0 - 6.0 - 0.40 - 0.65 - - - -
6 A194 410 S41000 1.4006 all size 228 to 271 20 to 28 - 0.15 max 1.00 0.04 0.03 1.00 11.5 - 13.5 - -  

Filter results
Select company type
by countries
SHARE
Wire and rods for oil and gas fasteners (ASTM A193, 194, A320)

Suppliers of Wire and rods for oil and gas fasteners (ASTM A193, 194, A320)

DETAILS
SEND YOUR REQUEST FOR QUOTATION
SEARCH RESULTS: 31
| 1 | 2 | 3 >  >>
GERMANY
VDM Metals Group

Manufacturer of sheet metal, strips, rods and wires in nickel, cobalt and zirconium alloys as well as high alloyed special stainless steels

INDIA
Resistant Metal Alloys LLP

Resistant Metal Alloys LLP is an exclusive Brand name for High Precision Build Fasteners in High Tensile, Corrosion Resistant Alloys, High Performance Alloys, Rare Exotic Alloys, Marine Alloys & ASTM / ASME Fasteners. It is engaged in manufacturing, stock holding and outsourcing Industrial Fasteners & providing traditional and customised fastening solutions globally!

INFORMATION RESTRICTED TO THE REGISTERED USERS
UCRAINA
A...

Distributor of high-quality metals and special alloys, non-ferrous metals, rare alloys

INFORMATION RESTRICTED TO THE REGISTERED USERS
ITALY
A...

Manufacturer of drawn wire coils, wire rods and bars. Materials: Stainless steels, super stainless steels, nickel alloys, superalloys and titanium.

INFORMATION RESTRICTED TO THE REGISTERED USERS
USA
A...

Manufacturer of titan and special metals

INFORMATION RESTRICTED TO THE REGISTERED USERS
USA
A...

Manufacturer of nickel alloy wire, bars and wire rope (Inconel, Hastelloy, Incoloy, Titanium, Duplex, Super Duplex, Stainless steel)

INFORMATION RESTRICTED TO THE REGISTERED USERS
INDIA
A...

Manufacturer of pipes, flanges, bars, sheets, wire rods in stainless steel, high nickel alloys and non-ferrous materials

INFORMATION RESTRICTED TO THE REGISTERED USERS
CHINA
B...

Manufacturer of raw material in titanium, zirconium and nickel. ASTM and ASM norms.

INFORMATION RESTRICTED TO THE REGISTERED USERS
CHINA
B...

Manufacturer of stainless steel, duplex and super alloys: tubes, pipes, plates, sheets, coils, strips, bars and rods

INFORMATION RESTRICTED TO THE REGISTERED USERS
GERMANY
B...

Manufacturer of stainless steel and superalloys. Forged products,  Semifinished products,  Bars, Wire rod,  Bright Steel, fien wire

CERTIFICATIONS: ISO 9001:2008 | 50001:2011 | ISO/TS 16949-2009